Електроди зварювальні Monolith ЭА-395/9

AWS A5.4: E308L-16
EN ISO 3581-A-Е Z 20 25 5 Cu N L В 2 2
CONDITIONS OF USE
  • applied when welding in all spatial positions, except from top to bottom, with a constant current of reverse polarity
  • welding must be performed with a short arc, without transverse oscillations, the edges should be cleaned before welding
SPECIAL PROPERTIES
  • very high reserve of austenity (EA-3)
  • excellent mechanical properties of the deposited metal
  • high welding and technological properties, easy separation of the slag crust, and the formation of a seam with a smooth transition to the base metal
  • surfacing coefficient: 0.19...0.20 g/A•min
  • consumption of electrodes per 1 kg of deposited metal: 1.4...1.5 kg
EA-395/9 electrodes are designed for responsible welding structures made of alloyed steels of increased and high strength, heat-resistant and low-magnetic steels, steels of the type AK 23, AK 25, AK 27, as well as welding dissimilar steels.
Package Weight
First select diameter
Packaging data
Diameter, mm Length, mm Number of electrodes in a pack, pcs. Pack weight, kg
3.0 350 39…40 1.0
4.0 350 20…21 1.0
Package Weight
First select diameter
Type of coating
basic
Weld metal chemical composition, %
According to AWS A5.1 / Typical results
C
Carbon
0,08…0,12
Mn
Manganese
1,00…2,30
Si
Silicon
≤ 0,7
P
Phosphorus
≤ 0,030
S
Sulfur
≤ 0,020
Mo
Molybdenum
4,5…7,0
Cr
Chrome
13,5…17,0
Ni
Nickel
23…27
Weld metal mechanical properties
According to AWS A5.1 / Typical results
  • Tensile strength, MPa: ≥ 600
  • Yield strength, MPa: ≥ 400
  • Elongation, %: ≥ 30
  • Impact strength KCU +20 °C, J /cm² ≥ 100
Re-drying before welding
  • permissible moisture content in the coating before use no more than 0.3%
  • in case of wetting of the electrode coating above the norm - dry for 60 minutes at 250±10 °С
Welding parameters
Welding current strength, A for electrodes with a diameter of, mm
3.0 mm 4.0 mm
80-110 120-150
Welding should be carried out with a direct current of reverse polarity, "+" on the electrode with a voltage arc of 20...25V.
WELDING POSITIONS
PA
PB
PC
PF
PE
PD
Package Weight
First select diameter

My Cart

0
Total:
0 UAH