Електроди зварювальні Monolith М-316L

AWS A5.4: E316L-16
EN ISO 3581-А-E 19 12 3 L R 1 2
CONDITIONS OF USE
  • applied when welding in all spatial positions, except vertical from top to bottom
  • welding is recommended to be performed at the maximum possible speed without transverse oscillations of the electrode
SPECIAL PROPERTIES
  • high resistance to acids, as well as to general and intercrystalline corrosion at temperatures up to 400 °С
  • characterized by high welding and technological properties, stable arc burning, easy slag removal, and good seam formation with smooth transition to the base metal
  • surfacing coefficient: 0.17...0.20 g/A•min
  • consumption of electrodes per 1 kg of deposited metal: 1.5...1, 6 kg
Electrodes of the Monolith M-316L brand are intended for welding corrosion-resistant austenitic Cr-Ni-Mo steels, type AISI 316, AISI 318, AISI 316L, 1.4435, X2CrNiMo17-12-3, X2CrNiMo18-14-3, 00Cr17Ni14Mo3, S31600, etc., for parts operating at temperatures temperature up to 400°С. Electrodes are suitable for welding cat- tanks, containers and equipment for used oils, for coke chemical installations, equipment working in contact with the sea water, parts of equipment in chemical, textile and cellulose paper industry, as well as production equipment wool and artificial silk.
Package Weight
First select diameter
Packaging data
Diameter, mm Length, mm Number of electrodes in a pack, pcs. Pack weight, kg
2.5 350 43…46 1.0
3.0 350 30…32 1.0
3.2 350 28…31 1.0
4.0 350 18…19 1.0
Package Weight
First select diameter
Type of coating
rutile
Weld metal chemical composition, %
According to AWS A5.1 / Typical results
C
Carbon
≤ 0,04
Mn
Manganese
≤ 2,0
Si
Silicon
≤ 1,0
P
Phosphorus
≤ 0,030
S
Sulfur
≤ 0,025
Mo
Molybdenum
2,5…3,0
Cr
Chrome
17,0…20,0
Cu
Copper
≤ 0,75
Ni
Nickel
11,0…13,0
Weld metal mechanical properties
According to AWS A5.1 / Typical results
  • Tensile strength, MPa: ≥ 510
  • Yield strength, MPa: ≥ 320
  • Elongation, %: ≥ 25
  • Impact strength KV +20 ˚С, J ≥ 70
Re-drying before welding
  • permissible moisture content in the coating before use is no more than 0.2%
  • in case of wetting of the electrode coating above the norm - dry for 60 minutes at 400±10 °С
FERRITE NUMBER IN THE DEPOSITED METAL
5-15 FN
Welding parameters
Welding current strength, A for electrodes with a diameter of, mm
2.5 mm 3.0 mm 3.2 mm 4.0 mm
50-80 70-100 80-110 90-130
Welding should be carried out with a direct current of reverse polarity, "+" on an electrode with a voltage arc of 23...27 V or with an alternating current from a transformer with an open-circuit voltage of 50 V.
WELDING POSITIONS
PA
PB
PC
PF
PE
PD